| 廠家(產(chǎn)地) | 韓國大韓 |
|---|---|
| 牌號(hào) | SB9230 |
| 加工級別 | 注塑級,吹塑級 |
| 特性級別 | 耐水解,耐磨,耐老化,抗靜電 |
| 用途級別 | 薄膜級 |
| 銷售方式 | 品牌經(jīng)銷 |
| 類型 | 標(biāo)準(zhǔn)料 |
供應(yīng) PP SB9230 韓國大韓油 進(jìn)口原料 PP 


| PP SB9302 韓國大韓油化工業(yè)公司物性數(shù)據(jù) |
| 暫無此原料描述部分┄ |
| 性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測試方法 | 測試數(shù)據(jù) | 數(shù)據(jù)單位 | |
| 其它性能 | 密度 | --- | ASTM D-1505 | 0.91 | g/cm3 |
| 基本性能 | 熔體流動(dòng)速率 | --- | ASTM D-1238 | 2 | g/10min |
| 吸水性 | --- | ASTM D-570 | >0.01 | % | |
| 機(jī)械性能 | Mold Shrinkage (Linear) | --- | KPIC Method | 1.4~1.8 | % |
| 屈服拉伸強(qiáng)度 | --- | ASTM D-638 | 250 | kgf/cm2 | |
| 斷裂伸長率 | --- | ASTM D-638 | <500 | % | |
| 彎曲模量 | --- | ASTM D-790 | 12500 | kgf/cm2 | |
| 洛氏硬度 | --- | ASTM D-785 | 85 | R Scale | |
| 艾佐德沖擊強(qiáng)度(缺口) | --- | ASTM D-256 | 50 | kgfcm/cm | |
| 電氣性能 | 體積電阻率 | --- | ASTM D-257 | 1 | 1017Ω.Н |
| 介電常數(shù) | 1KHz | ASTM D-150 | 2.3 | --- | |
| 耗散(損耗)因數(shù) | 1KHz | ASTM D-150 | 2 | 10-4 | |
| 介電強(qiáng)度(短時(shí)間) | --- | ASTM D-14 | 40 | kv/m | |
| Arc Resistance | --- | ASTM D-495 | 130 | sec | |
| 熱 性 能 | Heat Conductivity | --- | KPIC Method | 3 | 10-4calcm/cmsec℃ |
| 維卡軟化點(diǎn) | --- | ASTM D-1525 | 152 | ℃ | |
| 熱變形溫度 | --- | ASTM D-648 | 100 | ℃ | |
| 比熱性 | --- | KPIC Method | 0.46 | Ш/g℃ | |